Bottom line: Pressure Advance compensates for extrusion lag during acceleration and deceleration, which cleans up corners and surface finish. It must be tuned after flow calibration and re-checked whenever speed or material changes. Too low a value leaves bulging corners; too high a value starves them.

What the setting does

StateSymptomDirection
Too lowBulging corners, lagIncrease slightly
CorrectConsistent cornersKeep
Too highThin corners, gapsDecrease slightly

Tuning order

  1. Calibrate flow and E steps first.
  2. Print a test model with stepped values.
  3. Compare corner bulge and thinning.
  4. Re-tune after changing speed.
  5. Re-tune after changing material.

Costly mistakes

  • Tuning before flow is correct.
  • Increasing the value until corners look sharp by eye only.
  • Not re-tuning after speed changes.
  • Ignoring material differences.
  • Judging surface without checking layer adhesion.

Buyer / engineer checklist

  • Is flow calibrated?
  • Are corners consistent?
  • Was it re-tuned after speed or material changes?
  • Are surface and layer strength both checked?
  • Are settings recorded per material?

Tell us the printer and material and we can help narrow the tuning range.Printing advice