Pinholes and voids come from moisture, under-extrusion, trapped air, poor layer bonding or contaminated material. Correct the extrusion chain before changing unrelated settings.

Check material

  • Dry the spool.
  • Measure diameter.
  • Inspect contamination.

Check process

Calibrate flow, check nozzle condition and stabilise temperature. Reduce speed if pressure cannot keep up.

Validate

  • Surface.
  • Cross-section.
  • Strength.
  • Dimensions.
SymptomCauseAction
Random holesMoistureDry
Regular voidsUnder-extrusionCalibrate
Dark specksContaminationClean
Weak layersTemperatureStabilise

Common engineering mistakes

  • Only increasing flow.
  • Ignoring moisture.
  • Changing everything.
  • Not inspecting the part.
  • Using one sample.

Buyer checklist

  • Is the filament dry?
  • Is flow calibrated?
  • Is nozzle clean?
  • Is temperature stable?
  • Are voids repeatable?

Send photos and material history through our support form.