Bottom line: moisture absorbed by nylon or PETG turns into steam inside the nozzle, creating bubbles, crackling and unstable flow. Drying and dry storage solve the cause; temperature adjustments only mask it. Drying must be followed by immediate sealing.

How it happens

StageProcess
AbsorptionMaterial takes up atmospheric moisture
HeatingWater vaporises in the melt
ExpansionBubbles form in the extrusion
RuptureSurface blisters, noise, defects

Practical drying

  • PA: 70–90 °C for 4–12 h, per TDS.
  • PETG: 60–70 °C for 4–6 h.
  • PC: 80–120 °C for 4–8 h.
  • Seal immediately after drying.
  • Print from a dry box for long jobs.

Costly mistakes

  • Raising temperature to hide the issue.
  • Leaving filament exposed after drying.
  • Over-drying at excessive temperature.
  • Not monitoring storage humidity.
  • Judging only by appearance.

Buyer / engineer checklist

  • Is the material dry?
  • Is it kept dry while printing?
  • Is storage humidity controlled?
  • Are drying cycles logged?
  • Was a test part compared?

Tell us the material and storage conditions and we can help define the drying cycle.Drying advice